Material 1.4944
Aleación y acero resistente a altas temperaturas
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
X6NiCrTiMoV26-15 | UNS S66286 | request |
Material Category: Aleación y acero resistente a altas temperaturas
Chemical Composition
C % | Si % | Mn % | P % | S % | Al % | B % | Cr % | Mo % | Ni % | Ti % | V % |
max 0,08 | max 1,00 | max 2,00 | max 0,020 | max 0,015 | max 0,3500 | 0,0030 - 0,0100 | 13,50 - 16,00 | 1,00 - 1,50 | 24,00 - 27,00 | 1,90 - 2,30 | 0,10 - 0,50 |
Product Specifications
DIN EN 2398 (06/2009)
DIN EN 4315 (03/2008)
DIN EN 4317 (03/2008)
DIN EN 4318 (03/2008)
- WL
Mechanical Properties
vergütet | |||||||
0,2% Dehngrenze (Rp0,2) | Zugfestigkeit (Rm) | Bruchdehnung (A 5,65) | Kerbschlagarbeit (DVM) | Zeitstandfestigkeit 1.000 h | Zeitstandfestigkeit 10.000 h | Warmfestigkeit | bei Temperatur |
~ 700 °C | |||||||
>= 635 N/mm² | 930 - 1.180 N/mm² | >= 12 % | >= 27 Joule | ~ 20 °C | |||
>= 559 N/mm² | ~ 200 °C | ||||||
>= 539 N/mm² | ~ 300 °C | ||||||
>= 520 N/mm² | ~ 400 °C | ||||||
>= 500 N/mm² | ~ 500 °C | ||||||
>= 481 N/mm² | ~ 579 N/mm² | ~ 451 N/mm² | ~ 550 °C | ||||
>= 451 N/mm² | ~ 441 N/mm² | ~ 304 N/mm² | ~ 600 °C | ||||
~ 314 N/mm² | ~ 206 N/mm² | ~ 650 °C | |||||
>= 314 N/mm² | ~ 206 N/mm² | ~ 118 N/mm² | ~ 700 °C | ||||
~ 118 N/mm² | ~ 54 N/mm² | ~ 750 °C | |||||
>= 78 N/mm² | ~ 800 °C |
Material request