Material 1.0501
acero térmico tratable
C 35 es un acero tratable con calor sin alear. Se utiliza principalmente para la ingeniería mecánica general.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
Material Category: acero térmico tratable
Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % | Mo % | Ni % |
0,32 - 0,39 | max 0,40 | 0,50 - 0,80 | max 0,045 | max 0,045 | max 0,40 | max 0,10 | max 0,40 |
Mechanical Properties
DIN EN 10083-2 Unlegierte Stähle. | ||||||||
normalgeglüht | Streckgrenze (Re) | Zugfestigkeit (Rm) | Bruchdehnung (A5,65) | bei Temperatur | ||||
<= 16 mm | >= 300 N/mm² | >= 550 N/mm² | >= 18 % | ~ 20 ° C | ||||
16 - 100 mm | >= 270 N/mm² | >= 520 N/mm² | >= 19 % | ~ 20 ° C | ||||
100 - 250 mm | >= 245 N/mm² | >= 500 N/mm² | >= 19 % | ~ 20 ° C |
DIN EN 10083-2 Vergütungsstähle. | ||||||||
Vergütet | Streckgrenze (Re) | Zugfestigkeit (Rm) | Bruchdehnung (A5,65) | Einschnürung (Z) | bei Temperatur | |||
<= 16 mm | >= 430 N/mm² | 630 - 780 N/mm² | >= 17 % | >= 40 % | ~ 20 ° C | |||
16 - 40 mm | >= 380 N/mm² | 600 - 750 N/mm² | >= 19 % | >= 40 % | ~ 20 ° C | |||
40 - 100 mm | >= 320 N/mm² | 550 - 700 N/mm² | >= 20 % | >= 40 % | ~ 20 ° C |