Material 1.0501
Heat-treatable steel
C 35 is an unalloyeed heat treatable steel. It is mainly being used for general mechanical engineering.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
Material Category: Heat-treatable steel
Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % | Mo % | Ni % |
0,32 - 0,39 | max 0,40 | 0,50 - 0,80 | max 0,045 | max 0,045 | max 0,40 | max 0,10 | max 0,40 |
Mechanical Properties
DIN EN 10083-2 Unlegierte Stähle. | ||||||||
normalgeglüht | Streckgrenze (Re) | Zugfestigkeit (Rm) | Bruchdehnung (A5,65) | bei Temperatur | ||||
<= 16 mm | >= 300 N/mm² | >= 550 N/mm² | >= 18 % | ~ 20 ° C | ||||
16 - 100 mm | >= 270 N/mm² | >= 520 N/mm² | >= 19 % | ~ 20 ° C | ||||
100 - 250 mm | >= 245 N/mm² | >= 500 N/mm² | >= 19 % | ~ 20 ° C |
DIN EN 10083-2 Vergütungsstähle. | ||||||||
Vergütet | Streckgrenze (Re) | Zugfestigkeit (Rm) | Bruchdehnung (A5,65) | Einschnürung (Z) | bei Temperatur | |||
<= 16 mm | >= 430 N/mm² | 630 - 780 N/mm² | >= 17 % | >= 40 % | ~ 20 ° C | |||
16 - 40 mm | >= 380 N/mm² | 600 - 750 N/mm² | >= 19 % | >= 40 % | ~ 20 ° C | |||
40 - 100 mm | >= 320 N/mm² | 550 - 700 N/mm² | >= 20 % | >= 40 % | ~ 20 ° C |