Material 2.4665
Nickellegierung
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
AlloyX | UNS N06002 | request |
Material Category: Nickellegierung
Chemical Composition
C % | Si % | Mn % | P % | S % | Al % | B % | Co % | Cr % | Cu % | Fe % | Mo % | Ni % | W % |
0,05 - 0,15 | max 1,00 | max 1,00 | max 0,020 | max 0,015 | max 0,5000 | max 0,0100 | 0,50 - 2,50 | 20,50 - 23,00 | max 0,50 | 17,00 - 20,00 | 8,00 - 10,00 | Rest | 0,20 - 1,00 |
Product Specifications
DIN 17744 (09/2002)
DIN 17750 (09/2002)
DIN 17752 (09/2002)
DIN 17753 (09/2002)
DIN EN 10088-1 (12/2014)
DIN EN 10302 (06/2008)
- WL
Mechanical Properties
lösungsgeglüht | |||
0,2% Dehngrenze (Rp0,2) | Zugfestigkeit (Rm] | Bruchdehnung (A5, 65) | bei Temperatur |
>= 270 N/mm² | >= 690 N/mm² | >= 30 % | ~ 20 ° C |
>= 260 N/mm² | ~ 100 ° C | ||
>= 245 N/mm² | ~ 200 ° C | ||
>= 230 N/mm² | ~ 300 ° C | ||
>= 215 N/mm² | ~ 400 ° C | ||
>= 200 N/mm² | ~ 500 ° C | ||
>= 195 N/mm² | ~ 550 ° C | ||
>= 190 N/mm² | ~ 600 ° C | ||
>= 180 N/mm² | ~ 700 ° C | ||
>= 165 N/mm² | ~ 800 ° C | ||
>= 140 N/mm² | ~ 900 ° C | ||
>= 80 N/mm² | ~ 1.000 ° C |