Material 2.4669
Nickellegierung
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
AlloyX750 | UNS N07750 | request |
Material Category: Nickellegierung
Chemical Composition
C % | Si % | Mn % | P % | S % | Al % | Co % | Cr % | Cu % | Fe % | Nb % | Ni % | Ti % |
max 0,08 | max 0,50 | max 1,00 | max 0,020 | max 0,015 | 0,4000 - 1,0000 | max 1,00 | 14,00 - 17,00 | max 0,50 | 5,00 - 9,00 | 0,700 - 1,200 | mind 70,00 | 2,25 - 2,75 |
Product Specifications
DIN EN 10088-1 (12/2014)
DIN EN 10269 (02/2014)
DIN EN 10302 (06/2008)
- WL
Mechanical Properties
ausgehärtet | |||
0,2% Dehngrenze (Rp0,2) | Zugfestigkeit (Rm) | Bruchdehnung (A5, 65) | bei Temperatur |
>= 630 N/mm² | >= 980 N/mm² | >= 8 % | ~ 20 ° C |
>= 790 N/mm² | >= 1.170 N/mm² | >= 15 % | ~ 20 ° C |
>= 620 N/mm² | ~ 100 ° C | ||
>= 610 N/mm² | ~ 200 ° C | ||
>= 760 N/mm² | ~ 200 ° C | ||
>= 601 N/mm² | ~ 300 ° C | ||
>= 746 N/mm² | ~ 300 ° C | ||
>= 592 N/mm² | ~ 400 ° C | ||
>= 732 N/mm² | ~ 400 ° C | ||
>= 582 N/mm² | ~ 500 ° C | ||
>= 715 N/mm² | ~ 500 ° C | ||
>= 573 N/mm² | ~ 600 ° C | ||
>= 692 N/mm² | ~ 600 ° C | ||
>= 642 N/mm² | ~ 700 ° C | ||
>= 415 N/mm² | ~ 800 ° C |