Material 1.4878
acero resistente al calor
El material 1.4878 es un acero austenítico resistente al calor. 1.4878 es resistente a incrustaciones de hasta 850 ° C / 1562 ° F. La resistencia en atmósferas oxidantes y reductoras es baja.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
X8CrNiTi18-10 X12CrNiTi18-9 | AISI 321H UNS S32109 | request |
Material Category: acero resistente al calor
Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % | Ni % | - |
max 0,10 | max 1,00 | max 2,00 | max 0,045 | max 0,015 | 17,00 - 19,00 | 9,00 - 12,00 | Ti >= 5xC <= 0,80 |
Mechanical Properties
DIN EN 10095 (12/2018 (05/1999)) Hitzebeständige Stähle und Nickellegierungen. | |||||
Zeitdehngrenze 1.000 h (Rp 1,0) | Zeitdehngrenze 10.000 h (Rp 1,0) | Zeitstandfestigkeit 1.000 h | Zeitstandfestigkeit 10.000 | Zeitstandfestigkeit 100.000 h | bei Temperatur |
~ 110 N/mm² | ~ 85 N/mm² | ~ 200 N/mm² | ~ 142 N/mm² | ~ 65 N/mm² | ~ 600 ° C |
~ 45 N/mm² | ~ 30 N/mm² | ~ 88 N/mm² | ~ 48 N/mm² | ~ 22 N/mm² | ~ 700 ° C |
~ 15 N/mm² | ~ 10 N/mm² | ~ 30 N/mm² | ~ 15 N/mm² | ~ 10 N/mm² | ~ 800 ° C |
Flacherzeugnisse | ||||
lösungsgeglüht | Bruchdehnung (A5, 65) | Probenlage | bei Temperatur | |
0,5 - 3 mm | >= 40 % | längs | ~ 20 ° C | |
0,5 - 3 mm | >= 40 % | quer | ~ 20 ° C | |
>= 3 mm | >= 40 % | längs | ~ 20 ° C | |
>= 3 mm | >= 40 % | quer | ~ 20 ° C | |
lösungsgeglüht | 0,2% Dehngrenze (Rp0,2) | 1% Dehngrenze (Rp1,0) | Zugfestigkeit (Rm) | Härte [HB] |
<= 75 mm | >= 190 N/mm² | >= 230 N/mm² | 500 - 720 N/mm² | <= 215 HB |
Langerzeugnisse | ||
lösungsgeglüht | Bruchdehnung (A5, 65) | bei Temperatur |
<= 25 mm | >= 40 % | ~ 20 ° C |