Material 1.4335
Acero inoxidable
El grado 1.4335 es un acero inoxidable austenítico. 1.4335 tiene un contenido muy bajo en carbono y azufre y es muy resistente en medios oxidados.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
X1CrNi25-21 | UNS S31002 ASTM A310LNAG | request |
Material Category: Acero inoxidable
Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % | Mo % | N % | Ni % |
max 0,02 | max 0,25 | max 2,00 | max 0,025 | max 0,010 | 24,00 - 26,00 | max 0,20 | max 0,100 | 20,00 - 22,00 |
Mechanical Properties
lösungsgeglüht | ||
0,2% Dehngrenze (Rp0,2) | bei Temperatur | |
>= 150 N/mm² | ~ 100 ° C | |
>= 140 N/mm² | ~ 150 ° C | |
>= 130 N/mm² | ~ 200 ° C | |
>= 120 N/mm² | ~ 250 ° C | |
>= 115 N/mm² | ~ 300 ° C | |
>= 110 N/mm² | ~ 350 ° C | |
>= 105 N/mm² | ~ 400 ° C |
Warmgewalztes Blech | |||||
lösungsgeglüht | |||||
0,2% Dehngrenze (Rp0,2) | 1% Dehngrenze (Rp1,0) | Zugfestigkeit (Rm) | Bruchdehnung (A5, 65) | Kerbschlagarbeit KV (ISO-V/Charpy-V) | Probenlage |
>= 200 N/mm² | >= 240 N/mm² | 470 - 670 N/mm² | >= 40 % | >= 90 Joule | längs |
Material request