Material 1.3817
Acero no magnetizable
El material 1.3817 es un acero resistente a la corrosión y al ácido 1.3817 no es magnético.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
Material Category: Acero no magnetizable
Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % | N % | Ni % |
0,30 - 0,50 | max 1,00 | 17,00 - 19,00 | max 0,060 | max 0,030 | 3,00 - 5,00 | max 0,100 | max 1,00 |
Mechanical Properties
DIN SEW 390 (11/1991) Nichtmagnetisierbare Stähle. | ||||||
Stabstahl | ||||||
abgeschreckt | 0,2% Dehngrenze (Rp0,2) | Zugfestigkeit (Rm) | Bruchdehnung (A5, 65) | Kerbschlagarbeit (ISO-V/Charpy-V) | Probenlage | bei Temperatur |
<= 100 mm | >= 280 N/mm² | 750 - 950 N/mm² | >= 35 % | >= 85 Joule | längs | ~ 20 ° C |
<= 100 mm | >= 20 % | >= 55 Joule | quer | ~ 20 ° C |
Flacherzeugnisse | ||||||
abgeschreckt | 0,2% Dehngrenze (Rp0,2) | Zugfestigkeit (Rm) | Bruchdehnung (A5, 65) | Kerbschlagarbeit (ISO-V/Charpy-V) | Probenlage | bei Temperatur |
<= 20 mm | >= 280 N/mm² | 750 - 950 N/mm² | >= 35 % | >= 85 Joule | längs | ~ 20 ° C |
<= 20 mm | >= 20 % | >= 55 Joule | quer | ~ 20 ° C |
Schmiedestücke | ||||||
abgeschreckt | 0,2% Dehngrenze (Rp0,2) | Zugfestigkeit (Rm) | Bruchdehnung (A5, 65) | Kerbschlagarbeit (ISO-V/Charpy-V) | Probenlage | bei Temperatur |
<= 100 mm | >= 280 N/mm² | 750 - 950 N/mm² | >= 35 % | >= 85 Joule | längs | ~ 20 ° C |
<= 100 mm | >= 20 % | >= 55 Joule | quer | ~ 20 ° C |