Material Category: Nickellegierung
Chemical Composition
C % | Si % | Mn % | P % | S % | Al % | B % | Co % | Cr % | Cu % | Fe % | Mo % | Nb % | Ni % | Ti % |
0,02 - 0,08 | max 0,35 | max 0,35 | max 0,015 | max 0,015 | 0,3000 - 0,7000 | 0,0020 - 0,0060 | max 1,00 | 17,00 - 21,00 | max 0,30 | Rest | 2,80 - 3,30 | 4,700 - 5,500 | 50,00 - 55,00 | 0,60 - 1,20 |
Product Specifications
DIN 17744 (09/2002)
DIN 17750 (09/2002)
DIN 17752 (09/2002)
DIN 17753 (09/2002)
DIN EN 10088-1 (12/2014)
DIN EN 10269 (02/2014)
DIN EN 10302 (06/2008)
DIN SE 201 (10/1992)
- WL
Mechanical Properties
DIN EN 10269 (02/2014) Stähle und Nickellegierungen für Befestigungselemente für den Einsatz bei erhöhten und/oder tiefen Temperaturen. | |||||
Stabstahl | |||||
weichgeglüht | 0,2% Dehngrenze (Rp0,2) | Zugfestigkeit (Rm] | Bruchdehnung (A5, 65) | Kerbschlagarbeit KV2 (ISO-V/Charpy-V) | bei Temperatur |
<= 160 mm | >= 1.030 N/mm² | >= 12 % | >= 12 J | ~ 20 ° C | |
<= 160 mm | >= 1.030 N/mm² | >= 12 J | ~ 20 ° C | ||
<= 160 mm | >= 880 N/mm² | ~ 300 ° C | |||
<= 160 mm | >= 865 N/mm² | ~ 400 ° C | |||
<= 160 mm | >= 860 N/mm² | ~ 500 ° C | |||
<= 160 mm | >= 860 N/mm² | ~ 600 ° C |