Material 1.7264
Case hardening steel
1.7264 is an alloyed carbon steel with a density of 7.8
This material is used for components subject to higher loads.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
Material Category: Case hardening steel
Applications
gears
waves
crankshafts
connecting rod
camshafts
Heat Treatment
Annealing at 680 - 700 C°
Carburizing at 840 - 880 C°
Core hardening at 820 - 850 C°
Surface layer hardening at 810 - 830 C°
Temper at 150 - 180 C°
Weldability
20CrMo5 is usually weldable.
Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % | Mo % |
0,18 - 0,23 | 0,15 - 0,35 | 0,90 - 1,20 | max 0,035 | max 0,035 | 1,10 - 1,40 | 0,20 - 0,30 |
Mechanical Properties
Stabstahl | |
behandelt auf Härtespanne | Härte [HB 30] |
<= 150 mm | 179 - 217 HB 30 |
weichgeglüht | Härte [HB 30] |
<= 217 HB 30 |
nach Einsatzhärtung, im Kern | Streckgrenze (Re) | Zugfestigkeit (Rm) | Bruchdehnung (A5, 65) | Einschnürung (Z) | Kerbschlagarbeit KV (ISO-V/Charpy-V) |
<= 11 mm | >= 735 N/mm² | 1.080 - 1.370 N/mm² | >= 7 % | >= 30 % | >= 27 Joule |
<= 30 mm | >= 685 N/mm² | 980 - 1.270 N/mm² | >= 8 % | >= 35 % | >= 27 Joule |
<= 63 mm | >= 540 N/mm² | 780 - 1.080 N/mm² | >= 10 % | >= 35 % |