Material 1.4980
High-temperature resisting steel and alloy
The material 1.4980 is a high-temperature steel. In the anneale condition, the structure austenite an carbides on. In the cured state, the structure is austenitic steels, carbides and intermetallic phases. Shal due the cure hardness and strength increases. This steel can be up to a maximum temperature of about 700 °C / 1292 °F aare used. Typical products from 1.4980 are, for example, connecting parts, wich are used in turbine construction.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
X6NiCrTiMoVB25-15-2 X5NiCrTi26-15 | AISI 660 UNS S66286 | SUH660 | request |
Material Category: High-temperature resisting steel and alloy
Chemical Composition
C % | Si % | Mn % | P % | S % | Al % | B % | Cr % | Mo % | Ni % | Ti % | V % |
0,03 - 0,08 | max 1,00 | 1,00 - 2,00 | max 0,025 | max 0,015 | max 0,3500 | 0,0030 - 0,0100 | 13,50 - 16,00 | 1,00 - 1,50 | 24,00 - 27,00 | 1,90 - 2,30 | 0,10 - 0,50 |
Mechanical Properties
vergütet | |||||||
0,2% Dehngrenze (Rp0,2) | Zugfestigkeit (Rm) | Bruchdehnung (A 5,65) | Kerbschlagarbeit (DVM) | Zeitstandfestigkeit 10.000 h | Zeitstandfestigkeit 100.000 h | Warmfestigkeit | bei Temperatur |
~ 580 °C | |||||||
>= 635 N/mm² | 930 - 1.180 N/mm² | >= 12 % | >= 27 Joule | ~ 20 °C | |||
>= 559 N/mm² | ~ 200 °C | ||||||
>= 539 N/mm² | ~ 300 °C | ||||||
>= 520 N/mm² | ~ 400 °C | ||||||
>= 500 N/mm² | ~ 500 °C | ||||||
>= 481 N/mm² | ~ 579 N/mm² | ~ 451 N/mm² | ~ 550 °C | ||||
>= 451 N/mm² | ~ 441 N/mm² | ~ 304 N/mm² | ~ 600 °C | ||||
~ 314 N/mm² | ~ 206 N/mm² | ~ 650 °C | |||||
>= 314 N/mm² | ~ 206 N/mm² | ~ 118 N/mm² | ~ 700 °C | ||||
~ 118 N/mm² | ~ 54 N/mm² | ~ 750 °C | |||||
>= 78 N/mm² | ~ 800 °C |
Material request