Material 1.4919
High-temperature resisting steel and alloy
The material 1.4919 is a austenitic stainless steel, this material is also alloyed with nitrogen and boron. The nitrogen and boron alloying elements improve the mechanical properties at elevated temperatures. The material is often used in power plant cnstruction.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
X6CrNiMoB17-12-2 X6CrNiMo17-13 | AISI 316H UNS S31609 | SUS316HFB SUS316HTB SUS316HTF SUS316HTP | request |
Material Category: High-temperature resisting steel and alloy
Chemical Composition
C % | Si % | Mn % | P % | S % | B % | Cr % | Mo % | N % | Ni % |
0,04 - 0,08 | max 1,00 | max 2,00 | max 0,035 | max 0,015 | 0,0015 - 0,0050 | 16,50 - 18,50 | 2,00 - 2,50 | max 0,100 | 10,00 - 13,00 |
Mechanical Properties
lösungsgeglüht | ||||||||
0,2% Dehngrenze (Rp0,2) | Zugfestigkeit (Rm) | Bruchdehnung (A 5,65) | Kerbschlagarbeit (DVM) | Kerbschlagarbeit KV (ISO-V/Charpy-V) | Zeitstandfestigkeit 10.000 h | Zeitstandfestigkeit 100.000 h | Warmfestigkeit | bei Temperatur |
>= 205 N/mm² | 490 - 690 N/mm² | >= 35 % | >= 96 Joule | >= 90 Joule | ~ 20 °C | |||
>= 177 N/mm² | ~ 100 °C | |||||||
>= 147 N/mm² | ~ 200 °C | |||||||
>= 127 N/mm² | ~ 300 °C | |||||||
>= 118 N/mm² | ~ 400 °C | |||||||
>= 108 N/mm² | ~ 500 °C | |||||||
>= 103 N/mm² | ~ 250 N/mm² | ~ 175 N/mm² | ~ 550 °C | |||||
>= 98 N/mm² | ~ 175 N/mm² | ~ 120 N/mm² | ~ 600 °C | |||||
>= 78 N/mm² | ~ 111 N/mm² | ~ 69 N/mm² | ~ 650 °C | |||||
~ 65 N/mm² | ~ 34 N/mm² | ~ 700 °C | ~ 700 °C | |||||
~ 42 N/mm² | ~ 20 N/mm² | ~ 750 °C |