Material 1.4841

Heat-resisting steel

The material 1.4841 is austenitic heat resistant steel. 1.4841 is scaling resistant up to a temperature of about 1150 °C / 2102 °F.

Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.

1.4841

Chemical Composition

C % Si % Mn % P % S % Cr % N % Ni %
max 0,20 1,50 - 2,50 max 2,00 max 0,045 max 0,015 24,00 - 26,00 max 0,100 19,00 - 22,00

 

Mechanical Properties

DIN EN 10095 (12/2018 (05/1999))
Hitzebeständige Stähle und Nickellegierungen.
Zeitdehngrenze 1.000 h (Rp 1,0) Zeitdehngrenze 10.000 h (Rp 1,0) Zeitstandfestigkeit 1.000 h Zeitstandfestigkeit 10.000 Zeitstandfestigkeit 100.000 h bei Temperatur
~ 105 N/mm² ~ 95 N/mm² ~ 170 N/mm² ~ 130 N/mm² ~ 80 N/mm² ~ 600 ° C
~ 50 N/mm² ~ 35 N/mm² ~ 90 N/mm² ~ 40 N/mm² ~ 18 N/mm² ~ 700 ° C
~ 23 N/mm² ~ 10 N/mm² ~ 40 N/mm² ~ 20 N/mm² ~ 7 N/mm² ~ 800 ° C
~ 10 N/mm² ~ 4 N/mm² ~ 20 N/mm² ~ 10 N/mm² ~ 3 N/mm² ~ 900 ° C
~ 3 N/mm²   ~ 5 N/mm²     ~ 1000 ° C
Stäbe
geglüht 0,2% Dehngrenze (Rp0,2) Zugfestigkeit (Rm) Härte [HB] bei Temperatur
>= 160 mm >= 230 N/mm² 550 - 750 N/mm² <= 223 HB ~ 20 ° C
Flacherzeugnisse
geglüht Bruchdehnung (A5, 65) Probenlage bei Temperatur
0,5 - 3 mm >= 28 % längs ~ 20 ° C
0,5 - 3 mm >= 28 % quer ~ 20 ° C
>= 3 mm >= 30 % längs ~ 20 ° C
>= 3 mm >= 30 % quer ~ 20 ° C
Langerzeugnisse  
geglüht Bruchdehnung (A5, 65) bei Temperatur
<= 160 mm >= 30 % ~ 20 ° C

Material request

Screenreader label
_4__________97N______
7X_____P____9_B___HC9
_2____X7I___W_9______
_6_____X____J_Y___TIJ
F9Y_________WRF______
* mandatory field
Screenreader label

Company

Five reasons that are in favor of BASEDO STEEL

Learn more

Services

A short overview of our services

Learn more

Questions?

Would you like to ask us about your specific demands?

Contact us