Material 1.4571
Stainless steel
Grade 1.4571 is an austenitic titanium stabilized stainless steel. 1.4571/316Ti got a good corrosion resistance as well as good mechanical properties. This steel grade is still often being used in Germany.Internationally 1.4404/316L is offten being used instead since itts corrosion resistance is the same but 1.4404 is way simpler to process.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
X6CrNiMoTi17-12-2 | AISI 316Ti UNS S31635 | X6CrNiMoTi1712 X6CrNiMoTi1712KG X6CrNiMoTi1712KW | SUS316Ti SUS316TiTB SUS316TiTP | request |
Material Category: Stainless steel
Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % | Mo % | Ni % | - |
max 0,08 | max 1,00 | max 2,00 | max 0,045 | max 0,015 | 16,50 - 18,50 | 2,00 - 2,50 | 10,50 - 13,50 | Ti 5xC <= 0,70 |
Mechanical Properties
lösungsgeglüht | 0,2% Dehngrenze (Rp0,2) / bei Temperatur | 1% Dehngrenze (Rp1,0) | Zugfestigkeit (Rm) | Bruchdehnung (A5, 65) | Einschnürung (Z) | Härte [HB 30] | Kerbschlagarbeit KV (ISO-V/Charpy-V) | Probenlage |
<= 160 mm | >= 40 % | >= 100 Joule | längs | |||||
160 - 250 mm | >= 30 % | >= 60 Joule | quer | |||||
<= 250 mm | >= 200 N/mm² | >= 235 N/mm² | 500 - 700 N/mm² | >= 50 % | <= 215 HB 30 | längs | ||
>= 127 N/mm² / ~ 550 ° C | ||||||||
>= 129 N/mm² / ~ 500 ° C | ||||||||
>= 131 N/mm² / ~ 450 ° C | ||||||||
>= 135 N/mm² / ~ 400 ° C | ||||||||
>= 140 N/mm² / ~ 350 ° C | ||||||||
>= 145 N/mm² / ~ 300 ° C | ||||||||
>= 155 N/mm² / ~ 250 ° C | ||||||||
>= 165 N/mm² / ~ 200 ° C | ||||||||
>= 175 N/mm² / ~ 150 ° C | ||||||||
>= 185 N/mm² / ~ 100 ° C |