Material 1.4438
Stainless steel
1.4438 is an austenitic stainless steel. The high content of molybdenum is responsible for its resistance to reducing acids as well as chloride containing mediums. This grade can often be found in the chmical plant industry.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
X2CrNiMo18-15-4 X2CrNiMo1864 | AISI 317L UNS S31703 | X2CrNiMo1815 | SUS317L SUS317LFB SUS317LTB SUS317LTP SUSF317L SUSY317L | request |
Material Category: Stainless steel
Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % | Mo % | N % | Ni % |
max 0,03 | max 1,00 | max 2,00 | max 0,045 | max 0,015 | 17,50 - 19,50 | 3,00 - 4,00 | max 0,100 | 13,00 - 16,00 |
Mechanical Properties
lösungsgeglüht | 0,2% Dehngrenze (Rp0,2) / bei Temperatur | 1% Dehngrenze (Rp1,0) | Zugfestigkeit (Rm) | Bruchdehnung (A5, 65) | Einschnürung (Z) | Härte [HB 30] | Kerbschlagarbeit KV (ISO-V/Charpy-V) | Probenlage |
<= 160 mm | >= 40 % | >= 100 Joule | längs | |||||
160 - 250 mm | >= 30 % | >= 60 Joule | quer | |||||
<= 250 mm | >= 200 N/mm² | >= 235 N/mm² | 580 - 700 N/mm² | >= 60 % | <= 215 HB 30 | längs | ||
>= 108 N/mm² / ~ 550 ° C | ||||||||
>= 110 N/mm² / ~ 500 ° C | ||||||||
>= 112 N/mm² / ~ 450 ° C | ||||||||
>= 115 N/mm² / ~ 400 ° C | ||||||||
>= 120 N/mm² / ~ 350 ° C | ||||||||
>= 127 N/mm² / ~ 300 ° C | ||||||||
>= 137 N/mm² / ~ 250 ° C | ||||||||
>= 147 N/mm² / ~ 200 ° C | ||||||||
>= 157 N/mm² / ~ 150 ° C | ||||||||
>= 172 N/mm² / ~ 100 ° C |
Material request