Material 1.4016
Stainless steel
The corrosion resistance of 1.4016 is lower than that of stainless austenitic grades. But due to its ferritic microstructure, 1.4016 is resistant to the effects of stress corrosion cracking. However, the use of 1.4016 is limited by its poor weldability.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
X6Cr17 | AISI 430 UNS S43000 | X8Cr17 | SUS430 SUS430TB SUS430TKA SUS430TKC SUS430TP SUSY430 | request |
Material Category: Stainless steel
Applications
Construction industry
Decorative purposes
Electronic equipment
Food industry
Mechanical engineering
Heat Treatment
The heat treatment that makes this steel particularly soft consists of holding at temperatures between 750 °C - 850 °C followed by air cooling. 850 °C must not be exceeded, as this grade is sensitive to embrittlement due to grain growth.
Weldability
- 1.4016 is difficult to weld
Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % |
max 0,08 | max 1,00 | max 1,00 | max 0,040 | max 0,015 | 16,00 - 18,00 |
Mechanical Properties
geglüht | 0,2% Dehngrenze (Rp0,2) bei Temperatur | Zugfestigkeit (Rm) | Bruchdehnung (A 5, 65) | Einschnürung (Z) | Härte [HB 30] | Probenlage |
<= 100 mm | >= 240 N/mm² | 400 - 630 N/mm² | >= 20 % | >= 60 % | <= 200 HB 30 | längs |
>= 220 N/mm² / ~ 100 ° C | ||||||
>= 215 N/mm² / ~ 150 ° C | ||||||
>= 210 N/mm² / ~ 200 ° C | ||||||
>= 205 N/mm² / ~ 250 ° C | ||||||
>= 200 N/mm² / ~ 300 ° C | ||||||
>= 195 N/mm² / ~ 350 ° C | ||||||
>= 190 N/mm² / ~ 400 ° C |