Material 1.2603
Hot work tool steel
The tool steel 1.2603 has a high tempering resistance paired with a good heat wear resistance. 1.2603 has no problems with rapid temperature fluctuations. From 1.2603 extrusion tools are often made.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
45CrMoW5-8 | request |
Material Category: Hot work tool steel
Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % | Mo % | V % | W % |
0,40 - 0,50 | 0,50 - 0,70 | 0,30 - 0,50 | max 0,035 | max 0,035 | 1,30 - 1,60 | 0,40 - 0,60 | 0,75 - 0,90 | 0,40 - 0,60 |
Mechanical Properties
gebrauchsfestigkeit | 1.270 - 1.670 N/mm² | ||
Abkühlung mit | Mildes Wasser | Öl | Luft |
geglüht | Härte (HB 30) | <= 240 HB 30 |
gehärtet | Zugfestigkeit (Rm) | ~ 1.860 N/mm² |
angelassen bei ~ 400 ° C | Zugfestigkeit (Rm) | ~ 1.720 N/mm² |
angelassen bei ~ 450 ° C | Zugfestigkeit (Rm) | ~ 1.700 N/mm² |
angelassen bei ~ 500 ° C | Zugfestigkeit (Rm) | ~ 1.690 N/mm² |
angelassen bei ~ 550 ° C | Zugfestigkeit (Rm) | ~ 1.710 N/mm² |
angelassen bei ~ 600 ° C | Zugfestigkeit (Rm) | ~ 1.670 N/mm² |
angelassen bei ~ 650 ° C | Zugfestigkeit (Rm) | ~ 1.520 N/mm² |
angelassen bei ~ 700 ° C | Zugfestigkeit (Rm) | ~ 1.180 N/mm² |
Material request