Material 1.2367
Hot work tool steel
The tool steel 1.2367 is a hot-work steel with high wear resistance, good heat resistance and good resistance tempering. 1.2367 can be well cured. Frequently the material is used in the production of large die casting. Usually 1.2367 is delivered in the soft annealed condition.
Do you have any questions about the material or would you like to order? Complete our inquiry form, it`s free of charge and without obligation. We will get in touch with you in order to provide you with more information.
Standards
HDIN / EN | US-Standard | AFNOR | UNI | JIS | request |
---|---|---|---|---|---|
X38CrMoV5-3 | request |
Material Category: Hot work tool steel
Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % | Mo % | V % |
0,35 - 0,40 | 0,30 - 0,50 | 0,30 - 0,50 | max 0,030 | max 0,020 | 4,80 - 5,20 | 2,70 - 3,20 | 0,40 - 0,60 |
Mechanical Properties
DIN EN ISO 4957 Werkzeugstähle. Legierte Werkzeugstähle für Warmarbeit. | |
geglüht | <= 229 HBW |
gehärtet | ~ 56 HRC |
angelassen bei ~ 50 ° C | ~ 55,8 HRC |
angelassen bei ~ 100 ° C | ~ 55 HRC |
angelassen bei ~ 150 ° C | ~ 53,9 HRC |
angelassen bei ~ 200 ° C | ~ 52,5 HRC |
angelassen bei ~ 250 ° C | ~ 51,9 HRC |
angelassen bei ~ 300 ° C | ~ 51,9 HRC |
angelassen bei ~ 350 ° C | ~ 52,1 HRC |
angelassen bei ~ 400 ° C | ~ 53 HRC |
angelassen bei ~ 450 ° C | ~ 53,8 HRC |
angelassen bei ~ 500 ° C | ~ 54,1 HRC |
angelassen bei ~ 550 ° C | ~ 53,9 HRC |
angelassen bei ~ 600 ° C | ~ 51,8 HRC |
angelassen bei ~ 650 ° C | ~ 45,9 HRC |
angelassen bei ~ 700 ° C | ~ 35 HRC |
gehärtet und angelassen | <= 249 HBW |
>= 50 HRC |
Material request