Chemical Composition
C % | Si % | Mn % | P % | S % | Cr % | Mo % | V % |
0,48 - 0,53 | 0,80 - 1,10 | 0,20 - 0,40 | max 0,030 | max 0,030 | 4,80 - 5,20 | 1,25 - 1,45 | 0,80 - 1,00 |
Mechanical Properties
DIN EN ISO 4957 | ||
gebrauchshärte (HRC) | Wert | ~ 58 HRC |
geglüht | Härte (HBW) | <= 229 HB 30 |
gehärtet | Zugfestigkeit (Rm) | ~ 60 HRC |
angelassen bei ~ 400 ° C | Zugfestigkeit (Rm) | ~ 2.000 N/mm² |
angelassen bei ~ 450 ° C | Zugfestigkeit (Rm) | ~ 2.100 N/mm² |
angelassen bei ~ 500 ° C | Zugfestigkeit (Rm) | ~ 2.170 N/mm² |
angelassen bei ~ 550 ° C | Zugfestigkeit (Rm) | ~ 2.050 N/mm² |
angelassen bei ~ 600 ° C | Zugfestigkeit (Rm) | ~ 1.780 N/mm² |
angelassen bei ~ 650 ° C | Zugfestigkeit (Rm) | ~ 1.450 N/mm² |
angelassen bei ~ 700 ° C | Zugfestigkeit (Rm) | ~ 1.060 N/mm² |